Expandable-Mold Casting Processes with Expendable Patterns
-
Published:2008
Abstract
Depending on the size and application, castings manufactured with the expendable mold process and with expendable patterns increase the tolerance from 1.5 to 3.5 times that of the permanent pattern methods. This article reviews the two major expendable pattern methods, such as lost foam and investment casting. It discusses the Replicast casting process that involves patternmaking with polystyrene and a ceramic shell mold. The article contains a table that summarizes the differences in the steps of casting a part between the permanent pattern and expendable pattern methods.
Abstract
This article discusses the sequence of operations for producing a foam...
Sign in
ASM members
Member Sign InExpandable-Mold Casting Processes with Expendable Patterns, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.