Casting
Volume 15 is a comprehensive reference on the principles and practice of metal casting, covering the fundamentals, process selection and parameters, and materials performance. It addresses molten metal processing, solidification behavior, molding, foundry practice, and casting properties. It also describes the equipment and procedures commonly used in casting operations, along with their advantages and limitations. In addition, the volume provides information on process modeling, quality assurance, shape casting, die casting, expandable-mold and centrifugal casting, high-pressure cast irons, and liquid metal handling procedures. For information on the print version of Volume 15, ISBN 978-0-87170-711-6, follow this link.
Download citation file:
Table of Contents
-
Applications and Specification Guidelines
-
History and Trends of Metal CastingByThomas E. Prucha;Thomas E. PruchaAmerican Foundry SocietySearch for other works by this author on:Daniel Twarog;Daniel TwarogNorth American Die Casting AssociationSearch for other works by this author on:Raymond W. MonroeRaymond W. MonroeSteel Founders' Society of AmericaSearch for other works by this author on:Published:01 December 2008
-
Metalcasting Technology and the Purchasing ProcessPublished:01 December 2008
-
Casting Design Issues and Practices[1]ByH.W. StollH.W. StollNorthwestern UniversitySearch for other works by this author on:Published:01 December 2008
-
-
Principles of Liquid Metal Processing
-
Chemical Thermodynamics and KineticsByPublished:01 December 2008
-
Thermodynamic Properties of Iron-Base AlloysByDoru M. Stefanescu;Doru M. StefanescuOhio State UniversitySearch for other works by this author on:Published:01 December 2008
-
Gases in MetalsByRichard J. Fruehan;Richard J. FruehanCarnegie Mellon UniversitySearch for other works by this author on:Prince N. AnyalebechiPrince N. AnyalebechiGrand Valley State UniversitySearch for other works by this author on:Published:01 December 2008
-
Inclusion-Forming ReactionsByPaul K. TrojanPaul K. TrojanUniversity of Michigan—Dearborn; and Richard Fruehan, Carnegie Mellon University
Revising author
Search for other works by this author on:Published:01 December 2008
-
-
Melting and Remelting
-
Electric Arc Furnace Melting[1]ByJ.L. JorstadJ.L. JorstadJ.L.J. Technologies, Inc.Search for other works by this author on:Published:01 December 2008
-
Cupola FurnacesByWilliam L. Powell;William L. PowellThyssenKrupp-Waupaca
Retired
Search for other works by this author on:Alan P. Druschitz;Alan P. DruschitzUniversity of Alabama at BirminghamSearch for other works by this author on:Jim FrostJim FrostACIPCO Melting DepartmentSearch for other works by this author on:Published:01 December 2008 -
Induction FurnacesByRalph Y. PerkulRalph Y. PerkulFoundry Solutions & Design LLC
Revising author
Search for other works by this author on:Published:01 December 2008 -
Skull MeltingByG. KeoughG. KeoughConsarc
Revising author
Search for other works by this author on:Published:01 December 2008 -
Electron Beam MeltingByDavid W. TrippDavid W. TrippTIMET,USA
Revising author
Search for other works by this author on:Published:01 December 2008 -
Plasma Melting and HeatingByRobin Lampson;Robin LampsonRetech Systems
Revising author
Search for other works by this author on:Todd TelferTodd TelferRetech SystemsRevising author
Search for other works by this author on:Published:01 December 2008 -
Crucible FurnacesByGeorge GilesGeorge GilesMorgan Molten Metal SystemsSearch for other works by this author on:Published:01 December 2008
-
Reverberatory and Stack FurnacesPublished:01 December 2008
-
-
Molten Metal Processing and Handling
-
Transfer and Treatment of Molten Metal—An IntroductionPublished:01 December 2008
-
Molten-Metal FiltrationByRobert P. PischelRobert P. PischelFOSECO Metallurgical Inc.Search for other works by this author on:Published:01 December 2008
-
Aluminum Fluxes and Fluxing PracticeByPublished:01 December 2008
-
Modification of Aluminum-Silicon Alloys[1]ByG.K. SigworthG.K. SigworthAlcoa Primary MetalsSearch for other works by this author on:Published:01 December 2008
-
Grain Refinement of Aluminum Casting Alloys[1]ByPublished:01 December 2008
-
Refinement of the Primary Silicon Phase in Hypereutectic Aluminum-Silicon AlloysByJohn L. JorstadJohn L. JorstadJLJ Technologies, Inc.Search for other works by this author on:Published:01 December 2008
-
-
Principles of Solidification
-
Thermodynamics and Phase DiagramsByUrsula R. KattnerUrsula R. KattnerNational Institute of Standards and TechnologySearch for other works by this author on:Published:01 December 2008
-
Nucleation Kinetics and Grain Refinement[1]ByJ.H. PerepezkoJ.H. PerepezkoUniversity of Wisconsin—MadisonSearch for other works by this author on:Published:01 December 2008
-
Transport Phenomena During SolidificationByJonathan A. DantzigJonathan A. DantzigUniversity of Illinois at Urbana-ChampaignSearch for other works by this author on:Published:01 December 2008
-
Plane Front SolidificationByWilfried KurzWilfried KurzEcole Polytechnique Fédérale de Lausanne,SwitzerlandSearch for other works by this author on:Published:01 December 2008
-
Non-Plane Front SolidificationByRohit Trivedi;Rohit TrivediAmes Laboratory, USDOE and Iowa State UniversitySearch for other works by this author on:Erin SunseriErin SunseriAmes Laboratory, USDOE and Iowa State UniversitySearch for other works by this author on:Published:01 December 2008
-
Eutectic Solidification—An IntroductionBySumanth ShankarSumanth ShankarMcMaster UniversitySearch for other works by this author on:Published:01 December 2008
-
Solidification of Eutectic Alloys: Aluminum-SiliconByM.M. MakhloufM.M. MakhloufWorcester Polytechnic InstituteSearch for other works by this author on:Published:01 December 2008
-
Solidification of Eutectic Alloys: Cast Iron[1]ByAndreas Bührig-Polackzek;Andreas Bührig-PolackzekGießerei-InstitutSearch for other works by this author on:Daniel dos SantosDaniel dos SantosGießerei-InstitutSearch for other works by this author on:Published:01 December 2008
-
MicrosegregationByHarold D. BrodyHarold D. BrodyUniversity of ConnecticutSearch for other works by this author on:Published:01 December 2008
-
MacrosegregationByChristoph BeckermannChristoph BeckermannUniversity of IowaSearch for other works by this author on:Published:01 December 2008
-
Interpretation and Use of Cooling Curves—Thermal AnalysisByH. FredrikssonH. FredrikssonThe Royal Institute of Technology,SwedenSearch for other works by this author on:Published:01 December 2008
-
X-Ray Imaging of Solidification Processes and Microstructure EvolutionByRagnvald H. Mathiesen;Ragnvald H. MathiesenNorwegian University of Science and TechnologySearch for other works by this author on:Lars ArnbergLars ArnbergNorwegian University of Science and TechnologySearch for other works by this author on:Published:01 December 2008
-
The Oxide Film Defect: The BifilmByJohn CampbellJohn CampbellUniversity of Birmingham UKSearch for other works by this author on:Published:01 December 2008
-
Shrinkage Porosity and Gas PorosityByPublished:01 December 2008
-
Castability—Fluidity and Hot TearingByLars Arnberg;Lars ArnbergNorwegian University of Science and TechnologySearch for other works by this author on:Asbjørn MoAsbjørn MoSINTEF Materials and ChemistrySearch for other works by this author on:Published:01 December 2008
-
Semisolid Metal ProcessingByDiran ApelianDiran ApelianWorcester Polytechnic InstituteSearch for other works by this author on:Published:01 December 2008
-
Rapid SolidificationByW.J. BoettingerW.J. BoettingerNational Institute of Standards and TechnologySearch for other works by this author on:Published:01 December 2008
-
Solidification During Casting of Metal-Matrix CompositesByPradeep Rohatgi;Pradeep RohatgiUniversity of Wisconsin—MilwaukeeSearch for other works by this author on:Benjamin Schultz;Benjamin SchultzUniversity of Wisconsin—MilwaukeeSearch for other works by this author on:Nikhil Gupta;Nikhil GuptaPolytechnic Institute of New York UniversitySearch for other works by this author on:Atef DaoudAtef DaoudCentral Metallurgical Research and Development InstituteSearch for other works by this author on:Published:01 December 2008
-
Solidification Research in MicrogravityByMartin E. GlicksmanMartin E. GlicksmanUniversity of FloridaSearch for other works by this author on:Published:01 December 2008
-
HomogenizationBySujoy Krishna ChaudhurySujoy Krishna ChaudhuryHoneywell International, Inc.Search for other works by this author on:Published:01 December 2008
-
Heat TreatmentBySujoy Krishna ChaudhurySujoy Krishna ChaudhuryHoneywell International, Inc.Search for other works by this author on:Published:01 December 2008
-
Hot Isostatic Pressing of CastingsByStephen J. MashlStephen J. MashlBodycote HIP—North AmericaSearch for other works by this author on:Published:01 December 2008
-
-
Modeling and Analysis of Casting Processes
-
Modeling of Transport Phenomena and ElectromagneticsByMatthew John M. Krane;Matthew John M. KranePurdue UniversitySearch for other works by this author on:Vaughan R. Voller;Vaughan R. VollerUniversity of MinnesotaSearch for other works by this author on:Published:01 December 2008
-
Direct Modeling of Structure FormationByCh.-A. Gandin;Ch.-A. GandinEcole Nationale Superieure des Mines de ParisSearch for other works by this author on:I. SteinbachI. SteinbachRuhr-University BochumSearch for other works by this author on:Published:01 December 2008
-
Modeling of Microsegregation and MacrosegregationByJ.C. HeinrichJ.C. HeinrichUniversity of New MexicoSearch for other works by this author on:Published:01 December 2008
-
Modeling of Stress, Distortion, and Hot TearingByBrian G. Thomas;Brian G. ThomasUniversity of Illinois (UIUC)Search for other works by this author on:Michel BelletMichel BelletCentre de Mise en Forme des Matériaux (CEMEF)Search for other works by this author on:Published:01 December 2008
-
Practical Issues in Computer Simulation of Casting ProcessesByItsuo OhnakaItsuo OhnakaOsaka Sangyo University,JapanSearch for other works by this author on:Published:01 December 2008
-
Thermophysical PropertiesByJuan J. Valencia;Juan J. ValenciaConcurrent Technologies CorporationSearch for other works by this author on:Peter N. QuestedPeter N. QuestedNational Physical LaboratorySearch for other works by this author on:Published:01 December 2008
-
Principles and Practices of Shape Casting
-
Shape Casting Processes—An IntroductionByJ.L. JorstadJ.L. JorstadJ.L.J. Technologies, Inc.Search for other works by this author on:Published:01 December 2008
-
Patterns and PatternmakingByRobert C. VoigtRobert C. VoigtPennsylvania State UniversitySearch for other works by this author on:Published:01 December 2008
-
Casting Practice: Guidelines for Effective Production of Reliable CastingsByJohn CampbellJohn CampbellThe University of Birmingham,EnglandSearch for other works by this author on:Published:01 December 2008
-
Filling and Feeding System ConceptsByJohn CampbellJohn CampbellUniversity of Birmingham,EnglandSearch for other works by this author on:Published:01 December 2008
-
-
Expandable-Mold Casting Processes with Permanent Patterns
-
Introduction: Expendable Mold Processes with Permanent PatternsByBrian V. SmithBrian V. SmithGeneral Motors CorporationSearch for other works by this author on:Published:01 December 2008
-
Aggregates and Binders for Expendable MoldsByJohn Jorstad;John JorstadJ.L.J. Technologies, Inc.
Revising author
Search for other works by this author on:Mary Beth Krusiak;Mary Beth KrusiakSand Technology Co.Revising author
Search for other works by this author on:John O. Serra;John O. SerraCarpenter Brothers Inc.Revising author
Search for other works by this author on:Vic La FayVic La FayHill and GriffithRevising author
Search for other works by this author on:Published:01 December 2008 -
Shell Molding and Shell CoremakingByScott McIntyreScott McIntyreGrede Foundries, Inc
Revising author
Search for other works by this author on:Published:01 December 2008 -
Slurry MoldingByCharles D. Nelson;Charles D. NelsonMorris Bean and Company
Revising author
Search for other works by this author on:Wayne Rasmussen;Wayne RasmussenConsultantRevising author
Search for other works by this author on:John JorstadJohn JorstadJ.L.J. Technologies, Inc.Revising author
Search for other works by this author on:Published:01 December 2008
-
-
Expandable-Mold Casting Processes with Expendable Patterns
-
Introduction: Expendable Mold Processes with Expendable PatternsPublished:01 December 2008
-
Lost Foam CastingPublished:01 December 2008
-
Investment Casting[1]ByRobert A. HortonRobert A. HortonPrecision Metalsmiths, Inc.
Revising author
Search for other works by this author on:Published:01 December 2008
-
-
Centrifugal Casting
-
Centrifugal CastingBySufei Wei;Sufei WeiThe Centrifugal Casting Machine CompanySearch for other works by this author on:Published:01 December 2008
-
Horizontal Centrifugal Casting[1]ByY.V. MurtyY.V. MurtyCMI Inc.
Revising author
Search for other works by this author on:Published:01 December 2008 -
Vertical Centrifugal Casting[1]ByY.V. MurtyY.V. MurtyCMI Inc.
Revising author
Search for other works by this author on:Published:01 December 2008
-
-
Permanent Mold and Semipermanent Mold Processes
-
Permanent Mold CastingByDon Tyler;Don TylerGeneral Aluminum Manufacturing Co.
Revising author
Search for other works by this author on:Robert PischelRobert PischelFOSECO Metallurgical, Inc.Revising author
Search for other works by this author on:Published:01 December 2008 -
Low-Pressure Metal CastingByGregory G. Woycik;Gregory G. WoycikCMI Equipment and Engineering, Inc.Search for other works by this author on:Published:01 December 2008
-
Low-Pressure Countergravity CastingByGary SchollGary SchollMetal Casting Technology, Inc.Search for other works by this author on:Published:01 December 2008
-
-
High-Pressure Die Casting
-
High-Pressure Die CastingByWilliam A. ButlerWilliam A. ButlerGeneral Motors (Retired), Consultant for NADCASearch for other works by this author on:Published:01 December 2008
-
Hot Chamber Die CastingByFrank E. GoodwinFrank E. GoodwinInternational Lead Zinc Research OrganizationSearch for other works by this author on:Published:01 December 2008
-
Cold Chamber Die CastingByRobert J. McInerney, IIRobert J. McInerney, IIBuhlerPrinceSearch for other works by this author on:Published:01 December 2008
-
Squeeze Casting[1]ByRathrindra DasGuptaRathrindra DasGuptaNational Science FoundationSearch for other works by this author on:Published:01 December 2008
-
Vacuum High-Pressure Die CastingByWilliam A. ButlerWilliam A. ButlerGeneral Motors, Consultant to NADCA
Retired
Search for other works by this author on:Published:01 December 2008 -
Die Casting ToolingByDaniel L. TwarogDaniel L. TwarogNADCA
Revising author
Search for other works by this author on:Published:01 December 2008 -
Automation in High-Pressure Die CastingByPublished:01 December 2008
-
-
Semisolid Casting
-
Semisolid Casting—Introduction and FundamentalsByDiran Apelian;Diran ApelianWorcester Polytechnic InstituteSearch for other works by this author on:John JorstadJohn JorstadJ.L.J. Technologies, Inc.Search for other works by this author on:Published:01 December 2008
-
ThixocastingByJustin HeimschJustin HeimschMadison Kipp CorporationSearch for other works by this author on:Published:01 December 2008
-
RheocastingByDiran Apelian;Diran ApelianWorcester Polytechnic InstituteSearch for other works by this author on:John JorstadJohn JorstadJ.L.J. Technologies, Inc.Search for other works by this author on:Published:01 December 2008
-
Thixomolding[1]ByPublished:01 December 2008
-
-
Cast Irons
-
Introduction to Cast Irons[1]ByGeorge M. GoodrichGeorge M. GoodrichStork Climax Research ServicesSearch for other works by this author on:Published:01 December 2008
-
Ductile Iron Castings[1]ByGeorge M. GoodrichGeorge M. GoodrichStork Climax Research ServicesSearch for other works by this author on:Published:01 December 2008
-
Malleable Iron CastingsByC.J. van EttingerC.J. van EttingerGieterij Doesburg
Revising author
Search for other works by this author on:Published:01 December 2008 -
White Iron and High-Alloyed Iron CastingsByRichard B. GundlachRichard B. GundlachStork Climax Research ServicesSearch for other works by this author on:Published:01 December 2008
-
High-Alloy Graphitic IronsByRichard B. GundlachRichard B. GundlachStork Climax Research ServicesSearch for other works by this author on:Published:01 December 2008
-
-
Steel Castings
-
Steel Continuous CastingByRobert D. PehlkeRobert D. PehlkeUniversity of MichiganSearch for other works by this author on:Published:01 December 2008
-
Steel Castings PropertiesByDavid PoweleitDavid PoweleitSteel Founders' Society of America
Revising author
Search for other works by this author on:Published:01 December 2008 -
Selection and Evaluation of Steel CastingsByDavid PoweleitDavid PoweleitSteel Founders Society of AmericaSearch for other works by this author on:Published:01 December 2008
-
Casting of Nonferrous Alloys
-
Dross, Melt Loss, and Fluxing of Light Alloy MeltsByDavid V. NeffDavid V. NeffMetaullics Systems Division, Pyrotek Inc.Search for other works by this author on:Published:01 December 2008
-
Aluminum Alloy Ingot Casting and Continuous ProcessesByElwin RooyElwin RooyElwin Rooy & AssociatesSearch for other works by this author on:Published:01 December 2008
-
Copper Continuous Casting[1]ByPublished:01 December 2008
-
Nonferrous Alloy Castings
-
Aluminum and Aluminum Alloy CastingsPublished:01 December 2008
-
Copper and Copper Alloy CastingsByMahi Sahoo;Mahi SahooCANMET—Materials Technology LaboratorySearch for other works by this author on:Harold T. MichelsHarold T. MichelsCopper Development AssociationSearch for other works by this author on:Published:01 December 2008
-
Zinc and Zinc Alloy CastingsByFrank E. GoodwinFrank E. GoodwinInternational Zinc AssociationSearch for other works by this author on:Published:01 December 2008
-
Cobalt and Cobalt Alloy CastingsPublished:01 December 2008
-
Nickel and Nickel Alloy Castings[1]BySelçuk KuyucakSelçuk KuyucakCANMET—MTL, Natural Resources CanadaSearch for other works by this author on:Published:01 December 2008
-
Titanium and Titanium Alloy CastingsByMustafa GucluMustafa GucluStanley Associates Inc.Search for other works by this author on:Published:01 December 2008
-
Zirconium and Zirconium Alloy CastingsByRichard C. SutherlinRichard C. SutherlinATI Wah Chang, An Allegheny Technologies CompanySearch for other works by this author on:Published:01 December 2008
-
Synthesis and Processing of Cast Metal-Matrix Composites and Their ApplicationsByPradeep K. Rohatgi;Pradeep K. RohatgiUniversity of Wisconsin-MilwaukeeSearch for other works by this author on:Nikhil Gupta;Nikhil GuptaPolytechnic Institute of New York UniversitySearch for other works by this author on:Atef DaoudAtef DaoudCentral Metallurgical Research and Development Institute (CMRDI)Search for other works by this author on:Published:01 December 2008
-
-
Quality Assurance, Nondestructive Evaluation, and Failure Analysis
-
Approaches to Measurement of Metal Quality[1]ByRathindra DasGuptaRathindra DasGuptaNational Science FoundationSearch for other works by this author on:Published:01 December 2008
-
Nondestructive Testing of Components[1]ByRathindra DasGuptaRathindra DasGuptaNational Science FoundationSearch for other works by this author on:Published:01 December 2008
-
Casting Fracture CharacteristicsPublished:01 December 2008
-
Casting Failure Analysis Techniques and Case StudiesByCraig BrownCraig BrownStork Technimet, Inc.Search for other works by this author on:Published:01 December 2008
-
Common Defects in Various Casting ProcessesByRathindra DasGuptaRathindra DasGuptaNational Science FoundationSearch for other works by this author on:Published:01 December 2008
-
Repair Welding of CastingsByRandall CounselmanRandall CounselmanOldenburg Group Inc.Search for other works by this author on:Published:01 December 2008
-
Quality Planning Tools and ProceduresPublished:01 December 2008
-
Maintenance, Repair, Alterations, and Storage of Patterns and ToolingByHenry BakemeyerHenry BakemeyerDie Casting Design and ConsultingSearch for other works by this author on:Published:01 December 2008
-
-
Process Design
-
Design and Geometry
-
Casting Design and Geometry[1]ByMichael GwynMichael GwynAdvanced Technology Institute and American Foundry Society Technical DepartmentSearch for other works by this author on:Published:01 December 2008
-
-
Reference Information