Introduction to Corrosion in the Nuclear Power Industry
By
Barry M. Gordon
Barry M. Gordon
Chair, Structural Integrity Associates, Inc.
Search for other works by this author on:
-
Published:2006
Page range:
339 - 340
Abstract
This article reviews a series of serious corrosion problems that have plagued the light water reactor (LWR) industry. It discusses the complex corrosion mechanisms involved, and the development of practical engineering solutions for their mitigation. The article contains tables that present the corrosion history of LWRs, and the ten most expensive operation and maintenance costs of corrosion for a particular reactor site.
You do not currently have access to this chapter.
Citation
Barry M. Gordon, Introduction to Corrosion in the Nuclear Power Industry, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 339–340, https://doi.org/10.31399/asm.hb.v13c.a0004223
Download citation file:
Related Book Content
Corrosion in Cold Climates
Corrosion: Environments and Industries
Maintenance
Practical Induction Heat Treating (Second Edition)
Corrosion of Zirconium Alloy Components in Light Water Reactors
Corrosion: Environments and Industries
Safety and Environmental Concerns in Using Sintering Atmospheres
Powder Metallurgy
Liquid Penetrant Inspection
Nondestructive Evaluation of Materials
Salt Bath Nitriding
Practical Nitriding and Ferritic Nitrocarburizing
Glossary of Corrosion-Related Terms
Corrosion: Understanding the Basics
Global Cost of Corrosion—A Historical Review
Corrosion: Materials
Introduction to Metallurgically Influenced Corrosion
Corrosion: Fundamentals, Testing, and Protection
Glossary of Terms
Corrosion in the Petrochemical Industry (Second Edition)