Corrosion: Environments and Industries
Corrosion of Structures
-
Published:2006
Abstract
This article discusses the generic situation of steel reacting with the environments found in structures. Two environments are specifically discussed: atmospheric and cementitious. The article describes the utility of different corrosion protection methods for atmospheric corrosion and cementitious systems. It presents examples of problems that have arisen in the corrosion performance of steel.
Sign in
ASM members
Member Sign InJohn E. Slater, Corrosion of Structures, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 1054–1066, https://doi.org/10.31399/asm.hb.v13c.a0004220