This article discusses the generic situation of steel reacting with the environments found in structures. Two environments are specifically discussed: atmospheric and cementitious. The article describes the utility of different corrosion protection methods for atmospheric corrosion and cementitious systems. It presents examples of problems that have arisen in the corrosion performance of steel.
John E. Slater, Corrosion of Structures, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 1054–1066, https://doi.org/10.31399/asm.hb.v13c.a0004220