Corrosion in the Mining and Mineral Industry Available to Purchase
-
Published:2006
Abstract
This article describes the corrosion of principal parts of mining equipment such as mine shafts, wire rope, rock bolts, and pump and piping systems. It discusses the diagnosis and prevention of various types of corrosion including uniform corrosion, pitting corrosion, crevice corrosion, erosion-corrosion, and intergranular corrosion. The article explains the corrosion in tanks, reactor vessels, cyclic loading machinery, and pressure leaching equipment.
B. Mishra, J.J. Pak, Corrosion in the Mining and Mineral Industry, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 1076–1082, https://doi.org/10.31399/asm.hb.v13c.a0004219