Corrosion by Hydrogen Fluoride and Hydrofluoric Acid
-
Published:2006
Abstract
This article provides the corrosion data for materials in hydrofluoric acid (HF) and anhydrous hydrogen fluoride (AHF). These materials include carbon and low-alloy steels, austenitic stainless steels, nickel-rich austenitic stainless steels, nickel and nickel-base alloys, copper alloys, precious metals, and non-metals. The article also discusses the hydrogen blistering and stress-corrosion cracking of carbon steels in high-temperature HF and AHF.
Herbert S. Jennings, Corrosion by Hydrogen Fluoride and Hydrofluoric Acid, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 690–703, https://doi.org/10.31399/asm.hb.v13c.a0004182