Inspection, Data Collection, and Management
-
Published:2006
Abstract
This article focuses on the aspects associated with inspection related to pressure vessels and pipework. These aspects include inspection policy, inspection planning and procedures, inspection strategy, inspection methodology, preparation for inspection, invasive inspection, internal visual inspection, and non-invasive inspection. Inspection execution, risk-based inspection, competence assurance of inspection personnel, inspection coverage, inspection periodicity, inspection anomaly criteria, assessment of fitness, and reporting requirements, are also discussed. The article addresses the data acquisition, reporting and trending, and review and audit for the inspection. It reviews inspection techniques, including visual inspection, ultrasonic inspection, and radiographic inspection.
Sam McFarland, Inspection, Data Collection, and Management, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 1037–1053, https://doi.org/10.31399/asm.hb.v13c.a0004215
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.