Corrosion: Environments and Industries
Abstract
Understanding the high-temperature corrosion behavior of alloys is an important step toward the selection of appropriate alloys for process equipment. This article briefly describes the high-temperature corrosion modes that are frequently encountered in the chemical process industry. These modes include oxidation, carburization, metal dusting, nitridation, halogen corrosion, and sulfidation.
George Y. Lai, Corrosion in High-Temperature Environments, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 754–761, https://doi.org/10.31399/asm.hb.v13c.a0004189