Corrosion in the Military Available to Purchase
-
Published:2006
Abstract
This article reviews corrosion problems in the U.S. Department of Defense (DoD) and discusses management and maintenance aspects of the practices that address the cost and readiness. It describes the plans to institute corrosion prevention and control strategies under DoD directives in engineering design, material selection, and fabrication processes for new acquisitions. The article also suggests a long-term strategy to reduce the cost of corrosion control.
Vinod S. Agarwala, Corrosion in the Military, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 126–135, https://doi.org/10.31399/asm.hb.v13c.a0004119