Corrosion: Environments and Industries
Corrosion by Sulfuric Acid
-
Published:2006
Abstract
This article describes the selection of materials for the production and handling equipment of concentrated sulfuric acid, depending on factors such as the allowable corrosion rate, desired mechanical and physical properties, fabrication requirements, availability, and cost. Materials such as carbon steel, cast irons, austenitic stainless steels, higher austenitic stainless steels, higher chromium Fe-Ni-Mo alloys, nickel-base alloys, non-metals, and specific other metals and alloys are also discussed.
Sign in
ASM members
Member Sign InS.K. Brubaker, Corrosion by Sulfuric Acid, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 659–667, https://doi.org/10.31399/asm.hb.v13c.a0004178
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.