U.S. Navy Aircraft Corrosion
-
Published:2006
Abstract
This article describes the influences of the operational environments of U.S. Navy aircraft during corrosion-control process. The most widely used materials in airframe structures and components, such as aluminum, steel, titanium, and magnesium alloy systems, are reviewed. The article provides information on the inspections steps, corrosion-control issues, and corrosion-prevention strategies for naval aircraft. It contains a table that lists typical locations of corrosion on the aircraft. The article also provides examples of aircraft corrosion damage.
Sign in
ASM members
Member Sign InJohn E. Benfer, U.S. Navy Aircraft Corrosion, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 184–194, https://doi.org/10.31399/asm.hb.v13c.a0004127
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.