Corrosion Rate Probes for Soil Environments Available to Purchase
-
Published:2006
Abstract
This article explores the use of the electrochemical and nonelectrochemical techniques for measuring the corrosion behavior of buried metals and the types of probes used. The electrical resistance technique is the main nonelectrochemical technique used for measuring corrosion rate. Electrochemical techniques discussed include linear polarization resistance, electrochemical noise, harmonic distortion analysis, electrochemical impedance spectroscopy, and hydrogen permeation. The principles of operation for the corrosion measuring techniques are described along with examples of their use in soils.
Bernard S. Covino, Jr., Sophie J. Bullard, Corrosion Rate Probes for Soil Environments, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 115–121, https://doi.org/10.31399/asm.hb.v13c.a0004117
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.