Abstract
This article describes the corrosion modes in a waste-to-energy boiler. It discusses the corrosion protection and alloy performance with an emphasis on two main areas of the boiler: furnace water walls and super heaters.
You do not currently have access to this chapter.
Citation
George Y. Lai, High-Temperature Corrosion in Waste-to-Energy Boilers, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 482–485, https://doi.org/10.31399/asm.hb.v13c.a0004157
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Introduction
High-Temperature Corrosion and Materials Applications
Registered Trademarks and Trademarks
High-Temperature Corrosion and Materials Applications
Challenges in Materials Applications for High-Temperature Service
High-Temperature Corrosion and Materials Applications
Corrosion by Halogen and Hydrogen Halides
High-Temperature Corrosion and Materials Applications
High-Temperature Corrosion of Beryllium and Beryllium Alloys
Beryllium Chemistry and Processing
High-Temperature Corrosion in Gasifiers
Corrosion: Environments and Industries
Corrosion of Nickel and Nickel-Base Alloys
Corrosion: Materials
Stress-Assisted Corrosion and Cracking
High-Temperature Corrosion and Materials Applications
Glossary of Terms: Corrosion
Corrosion: Fundamentals, Testing, and Protection
High-Temperature Corrosion-Related Failures
Failure Analysis and Prevention (2021 Edition)