This article focuses on the various types of corrosion-related failure mechanisms and their effects on passive electrical components. The types include halide-induced corrosion, organic-acid-induced corrosion, electrochemical metal migration, silver tarnish, fretting, and metal whiskers. The passive electrical components include resistors, capacitors, wound components, sensors, transducers, relays, switches, connectors, printed circuit boards, and hardware.