Rouging of Stainless Steel in High-Purity Water
-
Published:2006
Abstract
Materials of construction for equipment and piping in pharmaceutical processing plants must be resistant to corrosion from the high-purity water, the buffer solutions used in preparation of the products, and the cleaning solutions used to maintain the purity of the product. The primary water used in pharmaceutical production is water for injection (WFI). This article presents the steps for preparing WFI and discusses the effect of chlorides on stainless steel. It provides information on the passive layer of stainless steels and chromium-containing nickel alloys. The article provides information on the surface finish of pharmaceutical equipment. It discusses the classification of rouge and the characteristics of cast type 316L stainless steel. The article also explains how and when to perform cleaning and repassivation process on classes of rouge.
John C. Tverberg, Rouging of Stainless Steel in High-Purity Water, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 15–22, https://doi.org/10.31399/asm.hb.v13c.a0004103
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!