This article briefly describes water and steam chemistry, which influence the effect of corrosion in boilers. The appropriate control measures to prevent corrosion in boilers are also presented. The article provides a discussion on the common causes of fluid-side corrosion such as flow-accelerated corrosion, oxygen pitting, chelant corrosion, caustic corrosion, acid corrosion, organic corrosion, phosphate corrosion, hydrogen damage, and corrosion-assisted cracking.