Close-Interval Survey Techniques Available to Purchase
-
Published:2006
Abstract
A close-interval survey (CIS) is a series of structure-to-electrolyte direct current potential measurements performed at regular intervals for assessing the level of cathodic protection (CP) on pipelines and other buried or submerged metallic structures. This article describes the equipment required to perform the CIS. It provides a discussion on the activities that should be performed during the preparation and execution of the CIS. The dynamic stray current identification and compensation by CIS is discussed briefly. The article also explains various factors involved in the validation of CIS data. It concludes with information on CIS data interpretation.
Drew Hevle, Angel Kowalski, Close-Interval Survey Techniques, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 84–88, https://doi.org/10.31399/asm.hb.v13c.a0004112
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.