Introduction to Corrosion in Specific Environments
By
Stephen D. Cramer
Stephen D. Cramer
National Energy Technology Laboratory, U.S. Department of Energy
Search for other works by this author on:
-
Published:2006
Abstract
This article describes the various environments affecting corrosion performance, corrosion protection, and corrosion control. These include freshwater environments, marine environments, and underground environments. The article provides information on corrosion in military environments and specialized environments, representing less-well-known environments with more limited applications.
You do not currently have access to this chapter.
Citation
Stephen D. Cramer, Introduction to Corrosion in Specific Environments, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 5–7, https://doi.org/10.31399/asm.hb.v13c.a0004100
Download citation file:
Related Book Content
Corrosion in Cold Climates
Corrosion: Environments and Industries
Corrosion of Electronic Equipment in Military Environments
Corrosion: Environments and Industries
Designing to Minimize Corrosion
Corrosion: Fundamentals, Testing, and Protection
Corrosion in the Military
Corrosion: Environments and Industries
Corrosion in Service Water Distribution Systems
Corrosion: Environments and Industries
Glossary of Terms: Corrosion
Corrosion: Fundamentals, Testing, and Protection
Corrosion and Wear Control for Industrial Applications
Thermal Spray Technology
Corrosion in Petroleum Production Operations
Corrosion: Environments and Industries
Corrosion Control for Marine- and Land-Based Infrastructure Applications
Thermal Spray Technology
Waste-to-Energy Boilers and Waste Incinerators
High-Temperature Corrosion and Materials Applications