Corrosion in the Building Industries
-
Published:2006
Abstract
This article discusses the generic situation of steel reacting with the environments found in structures. Two environments are specifically discussed: atmospheric and cementitious. The article describes the utility of different corrosion protection methods for atmospheric corrosion and cementitious systems. It presents examples of problems that have arisen in the corrosion performance of steel.
You do not currently have access to this chapter.
Citation
Corrosion in the Building Industries, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Publication History
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Foreword
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Preface
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Credits
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Publication History
Engineered Materials Handbook Desk Edition