Corrosion in the Petroleum and Petrochemical Industry
-
Published:2006
Abstract
This article discusses the particular corrosion problems encountered and the corrosion control methods used in petroleum production (i.e., upstream) and the storage and transportation of oil and gas (i.e., midstream) up to the refinery (i.e., downstream). These control methods include proper material selection, protective coatings, cathodic protection systems, use of inhibitors, use of nonmetallic materials, and control of the environment. The article reviews the aspects of corrosion that tend to be unique to corrosion as encountered in applications involving oil and gas exploration and production. It discusses corrosion problems that are specific to the various types of environments or...
Sign in
ASM members
Member Sign InCorrosion in the Petroleum and Petrochemical Industry, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.