Corrosion in the Pharmaceutical and Medical Technology Industries
-
Published:2006
Abstract
This article discusses the corrosion characteristics of superaustenitic stainless and duplex stainless steels, which are used in pharmaceutical industry. It describes passivation treatments and the electropolishing of stainless steels. The article informs that electropolishing is not a passivation treatment, although the proper execution of the process will result in a passive surface. The article concludes with a discussion on roughing, which is a phenomenon of particular interest to the pharmaceutical industry.
Abstract
This article discusses the materials of construction found in pharmaceutical production facilities. The materials discussed are different stainless steels, nickel and nickel-base alloys, titanium, zirconium, impervious graphite,...
Sign in
ASM members
Member Sign InCorrosion in the Pharmaceutical and Medical Technology Industries, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.