This article addresses several distinct aspects of corrosion that should be taken into account when solving the corrosion problems in the food and beverage industries. It summarizes the role of international standards in developing food and beverage industries: the American Society of Mechanical Engineers (ASME), American Welding Society (AWS), and Food and Drug Administration (FDA). The article tabulates the approximate pH values of various foods. It describes the contamination of food products by corrosion. A discussion on specific stainless steels, their corrosion resistance, fabrication, and applications is presented and compared to other potential materials of construction. The article also...
Sign in
ASM members
Member Sign InCorrosion in the Food and Beverage Industries, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.