Corrosion in the Chemical Processing Industry
-
Published:2006
Abstract
This article focuses on the effects of process variables on corrosion of metals in processing plants: plant environments; startup, shutdown, and downtime conditions; and seasonal temperature changes. It also tabulates the effects of process variables on corrosion of metals in aggressive environments.
Abstract
This article provides a detailed discussion on the corrosion of steel and stainless steel under insulation. Stress corrosion cracking mechanism, types of alloys susceptible to corrosion, factors influencing corrosion, and corrosion prevention methods, are also discussed.
Abstract
This article describes the selection of materials for the production and handling equipment of concentrated sulfuric acid, depending on...
Sign in
ASM members
Member Sign InCorrosion in the Chemical Processing Industry, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.