Corrosion: Environments and Industries
Corrosion in the Microelectronics Industry
-
Published:2006
Abstract
This article discusses the influence of the materials, design, package type, and environment on corrosion in microelectronics. It describes the common sources and mechanisms of corrosion in microelectronics, including anodic, cathodic, and electrolytic reactions resulting in uniform corrosion, galvanic corrosion, pitting corrosion, creep corrosion, dendrite growth, fretting, stress-corrosion cracking, and whisker growth. The article presents effective measures for minimizing the moisture retention in hermetic packages and/or moisture ingress in plastic packages. It concludes with information corrosion tests.
Abstract
This article presents a detailed examination of corrosion at the various production stages of wafer fabrication. The corrosion issues related to...
Sign in
ASM members
Member Sign InCorrosion in the Microelectronics Industry, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.