This article reviews corrosion problems in the U.S. Department of Defense (DoD) and discusses management and maintenance aspects of the practices that address the cost and readiness. It describes the plans to institute corrosion prevention and control strategies under DoD directives in engineering design, material selection, and fabrication processes for new acquisitions. The article also suggests a long-term strategy to reduce the cost of corrosion control.

This article provides a perspective on United States (U.S.) Department of Defense (DOD) specifications, standards, handbooks, and related documents, as well as their role in the corrosion prevention and control activities in the U.S. military.