This article is a pictorial guide to forms of corrosion that draws attention to common pitfalls or situations that have caused premature corrosion, sometimes with expensive consequences. The examples used are not exhaustive; they highlight the necessity to fully examine materials, conditions, and specific circumstances that together can reduce the anticipated service life of a component or plant. The color images in this article are categorized according to the type of corrosion following the general order that is adopted in Volume 13A of ASM Handbook. The first table of the article provides a categorization of the forms of corrosion. It also provides a reference to articles or sections of articles in Volume 13A that detail the particular corrosion form or mechanism. The second table is a guide listing the figures in this article by material and by the corrosion form or mechanism illustrated.
Peter Elliott, Gallery of Corrosion Damage, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 631–646, https://doi.org/10.31399/asm.hb.v13b.a0003969
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!