Introduction to Environmental Performance of Nonmetallic Materials
By
David C. Silverman
David C. Silverman
Argentum Solutions, Inc.
Search for other works by this author on:
-
Published:2005
Abstract
This article provides an overview of the environmental performance of the most commonly used nonmetallic materials, including elastomers, plastics, thermosetting resins, resin-matrix composites, organic coatings, concrete, refractories, and ceramics. It also discusses the applications and uses of these materials.
You do not currently have access to this chapter.
Citation
David C. Silverman, Introduction to Environmental Performance of Nonmetallic Materials, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 545–546, https://doi.org/10.31399/asm.hb.v13b.a0003840
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Property Comparison Tables: Hardness and Tensile Properties
Mechanical Testing and Evaluation
Tribology of Plastics and Elastomers
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Mechanical Testing and Properties of Plastics—An Introduction
Characterization and Failure Analysis of Plastics
Corrosion in Petroleum Production Operations
Corrosion: Environments and Industries
Hardness Measurement of Plastics and Elastomers
Hardness Testing Principles and Applications
Mechanical Testing and Properties of Plastics: An Introduction
Characterization and Failure Analysis of Plastics
Glossary of Terms: Mechanical Testing and Evaluation
Mechanical Testing and Evaluation
Electrical Testing of Polymers
Engineered Materials Handbook Desk Edition
Materials Issues in Joining
Joining Understanding the Basics
Corrosion in Petroleum Production Operations
Corrosion in the Petrochemical Industry (Second Edition)