Abstract
This article examines the high-temperature oxidation of silica-forming ceramics under constant temperature and cyclic conditions. The effects of water vapor, impurities, and molten salts are discussed. The article describes the oxidation and corrosion of silica-forming composites, oxide ceramics, non-silica forming nitrides, carbides, and borides. The performance of environmental barrier coatings by material type is also discussed. The article also explains the effects of oxidation and corrosion on the mechanical properties of ceramic-matrix composites. It concludes with information on high-temperature applications, wear properties, and the microscopic analyses of advanced ceramics.
Nathan S. Jacobson, Dennis S. Fox, James L. Smialek, Elizabeth J. Opila, Christopher Dellacorte, Kang N. Lee, Performance of Ceramics in Severe Environments, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, p 565–578, https://doi.org/10.31399/asm.hb.v13b.a0003842
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.