Abstract
This article discusses the corrosion of chromium electrodeposits and the ways for optimizing corrosion resistance. It describes the processing steps and conditions for hard chromium plating. These steps include pretreatment, electroplating, and posttreatment. The article also provides information on duplex coatings and the applications of chromium electrodeposits.
You do not currently have access to this chapter.
Citation
Allen R. Jones, Corrosion of Electroplated Hard Chromium, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 434–441, https://doi.org/10.31399/asm.hb.v13b.a0003833
Download citation file:
Related Book Content
Corrosion of Metallic Coatings
Corrosion: Environments and Industries
Corrosion in the Food and Beverage Industries
Corrosion: Environments and Industries
Corrosion Resistance of Stainless Steels and Nickel Alloys
Corrosion: Fundamentals, Testing, and Protection
Tin and Tin Alloys
Metals Handbook Desk Edition (2nd Edition)
Surface Engineering to Add a Surface Layer or Coating
Surface Engineering for Corrosion and Wear Resistance
Corrosion of Brazed and Soldered Joints
Corrosion: Materials
Decorative Chromium Plating
Surface Engineering
Fatigue Failure of a Diesel Engine Crankshaft
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Surface Engineering
Thermal Spray Technology
Corrosion and Wear Control for Industrial Applications
Thermal Spray Technology