Corrosion of Electroplated Hard Chromium
-
Published:2005
Abstract
This article discusses the corrosion of chromium electrodeposits and the ways for optimizing corrosion resistance. It describes the processing steps and conditions for hard chromium plating. These steps include pretreatment, electroplating, and posttreatment. The article also provides information on duplex coatings and the applications of chromium electrodeposits.
Allen R. Jones, Corrosion of Electroplated Hard Chromium, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 434–441, https://doi.org/10.31399/asm.hb.v13b.a0003833