This article discusses a tool for the conversion of measurements made against various reference electrodes at different temperatures. It reviews different electrode potential temperature coefficients, namely, isothermal temperature coefficient and thermal temperature coefficient. The article contains a table that lists the electrode potentials and conversion factors for various reference electrodes.