Corrosion: Materials
Environmental Performance of Nonmetallic Materials
-
Published:2005
Abstract
This article provides an overview of the environmental performance of the most commonly used nonmetallic materials, including elastomers, plastics, thermosetting resins, resin-matrix composites, organic coatings, concrete, refractories, and ceramics. It also discusses the applications and uses of these materials.
Abstract
This article provides an overview of the corrosion theory relating to refractories on the basis of acid/base reactions, thermodynamics, and kinetic considerations. The tests to evaluate refractory corrosive wear are reviewed. The article describes the specific refractories used in steel, glass, aluminum, and chemical-resistant applications. Specific material issues that should be considered or evaluated when choosing or using refractory...
Sign in
ASM members
Member Sign InEnvironmental Performance of Nonmetallic Materials, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.