Ferrous metals are metals that contain primarily iron and may have small amounts of other elements added to give the desired properties. This article discuses the characteristics of steel products used in most industries, including construction, automotive, energy, shipping, and agriculture. These products include bars, rods, wires, hot and cold rolled sheets, strip plates, tin mill products, steel tubes, castings, and forgings. The article also provides information on the methods used to prevent or control the rusting of ferrous materials, namely, alloying, coating, and covering.

This article discusses the environmental factors and kinetics of atmospheric corrosion, aqueous corrosion, and soil corrosion of carbon steels. It also provides information on corrosion in concrete and steel boilers.