Health and safety are critically important issues, and there are numerous aspects of the production and use of metal powders that may entail exposure to hazardous conditions. This article provides a discussion on the issues associated with the safe production and handling of metal powders and the safe operation of continuous mesh belt sintering furnaces with combustible atmospheres. It also provides a comprehensive high-level overview of the safety-related issues and concerns related to the use of compacting presses in the manufacturing sector.