Cold Isostatic Pressing Available to Purchase
-
Published:2015
Abstract
This article describes the unique aspects of cold isostatic pressing (CIP) in comparison with die compaction, for powder metallurgy parts. It details the components of CIP equipment, including pressure vessels, pressure generators, and tooling material. The article reviews the part shapes and their influence in determining tap density of the filled mold. It provides a discussion on process parameters, such as dwell time, depressurization rate, evaluation of green strength and density, and thermal processing, and illustrates a process flowchart for the production of CIP parts.
Peter E. Price, Cold Isostatic Pressing, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 255–259, https://doi.org/10.31399/asm.hb.v07.a0006074