Secondary Operations for Powder Metallurgy Stainless Steels
-
Published:2015
Abstract
Powder metallurgy (PM) stainless steels, as with conventional PM steels, are often used in the as-sintered condition. In addition to cost considerations, minimization of postsinter handling and secondary operations is also preferred because it reduces the potential for contamination of the parts with particulates and residues, which can result in the appearance of surface rust. This article provides information on various secondary operations, including tumbling, re-pressing, resin impregnation, annealing or heat treating, brazing, machining, and welding. It describes those aspects relating to welding of PM stainless steels, specifically, the effects of density, residual porosity, and sintered chemistry on weldability....
Sign in
ASM members
Member Sign InPeter A dePoutiloff, Secondary Operations for Powder Metallurgy Stainless Steels, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 440–446, https://doi.org/10.31399/asm.hb.v07.a0006119
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.