Particle Image Analysis
By
Bo Hu
Bo Hu
North American Höganäs, Inc.
Search for other works by this author on:
-
Published:2015
Abstract
Particle image analysis of metal powders can be easily performed with optical macroscopes and microscopes. This article provides examples of the particle image analysis on powders used in the powder metallurgy industry.
You do not currently have access to this chapter.
Citation
Bo Hu, Particle Image Analysis, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 154–155, https://doi.org/10.31399/asm.hb.v07.a0006102
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Powder Metallurgy Methods and Applications
Powder Metallurgy
High-Temperature Sintering of Ferrous Powder Metallurgy Components
Powder Metallurgy
Modeling and Simulation of Press and Sinter Powder Metallurgy
Powder Metallurgy
Scanning Electron Microscopy
Materials Characterization
The Various Microstructures of Room-Temperature Steel
Steel Metallurgy for the Non-Metallurgist
Introduction to Characterization of Powders
Materials Characterization (2019 Edition)
Powder Metallurgy
Metals Fabrication Understanding the Basics
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Brief Glossary of Terms
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Friction Powder Metallurgy Materials
Powder Metallurgy