Skip Nav Destination
ASM Handbook
Powder Metallurgy
Edited by
ASM International
Volume
7
ISBN electronic:
978-1-62708-175-7
Publication date:
2015
Book Chapter
Particle Image Analysis
By
Bo Hu
Bo Hu
North American Höganäs, Inc.
Search for other works by this author on:
-
Published:2015
Page range:
154 - 155
Abstract
Particle image analysis of metal powders can be easily performed with optical macroscopes and microscopes. This article provides examples of the particle image analysis on powders used in the powder metallurgy industry.
You do not currently have access to this chapter.
Citation
Bo Hu, Particle Image Analysis, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 154–155, https://doi.org/10.31399/asm.hb.v07.a0006102
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Powder Metallurgy Methods and Applications
Powder Metallurgy
High-Temperature Sintering of Ferrous Powder Metallurgy Components
Powder Metallurgy
Modeling and Simulation of Press and Sinter Powder Metallurgy
Powder Metallurgy
Evolution of Powder Metallurgy
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Appendix
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Introduction to Characterization of Powders
Materials Characterization (2019 Edition)
Scanning Electron Microscopy
Materials Characterization
Powder Metallurgy
Metals Fabrication Understanding the Basics
Dedication
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Preface
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements