Book Chapter
Introduction to Powder Metallurgy Stainless Steels Available to Purchase
-
Published:2015
Page range:
413 - 414
Abstract
Stainless steels are highly alloyed materials in comparison to most other popular powder metallurgy (PM) materials, such as low-alloy steels, copper alloys, and aluminum alloys. This article provides an overview of the history of PM stainless steels.
You do not currently have access to this chapter.
Citation
Prasan K. Samal, Introduction to Powder Metallurgy Stainless Steels, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 413–414, https://doi.org/10.31399/asm.hb.v07.a0006066
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Procedure Development and Practice Considerations for Ultrasonic Welding
Welding, Brazing, and Soldering
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Corrosion-Resistant Powder Metallurgy Alloys
Corrosion: Materials
Microbiologically Influenced Corrosion in Military Environments
Corrosion: Environments and Industries
Arc Welding
Metals Handbook Desk Edition (2nd Edition)
Forging of Specific Metals and Alloys
Metals Handbook Desk Edition (2nd Edition)
Corrosion by Organic Acids
Corrosion: Environments and Industries
Flux Cored Arc Welding
Welding Fundamentals and Processes
Procedure Development and Practice Considerations for Diffusion Welding
Welding, Brazing, and Soldering
Procedure Development and Practice Considerations for Resistance Welding
Welding, Brazing, and Soldering