Chemical Composition of Powder Metallurgy High-Alloy Tool Steels Available to Purchase
By
Paul Beiss
Paul Beiss
RWTH Aachen University
Search for other works by this author on:
-
Published:2015
Page range:
530 - 532
Abstract
This article is a comprehensive collection of tables that list the nominal chemical composition of common powder metallurgy (PM) high-alloy tool steels, namely, PM high-speed, cold working, and corrosion-resistant tool steels.
You do not currently have access to this chapter.
Citation
Paul Beiss, Chemical Composition of Powder Metallurgy High-Alloy Tool Steels, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 530–532, https://doi.org/10.31399/asm.hb.v07.a0006130
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Microstructure of Powder Metallurgy Tool Steels
Powder Metallurgy
Effects of Alloying on Powder Metallurgy Tool Steels
Powder Metallurgy
Properties of Powder Metallurgy Tool Steels
Powder Metallurgy
Evolution of Powder Metallurgy
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Appendix
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Powder Metallurgy
Metals Fabrication Understanding the Basics
Dedication
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Preface
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
About the Editors
Powder Metallurgy and Additive Manufacturing: Fundamentals and Advancements
Brief Glossary of Terms
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties