Abstract
Powder metallurgy (PM) high-alloy tool steels (HATS) have unique properties that assist them in solving various problems related to machining of metal components. This article describes the cost-intensive PM processing routes of HATS, as well as their major properties, including elastic properties, density, mechanical properties, grindability, fatigue and wear resistance, and thermophysical properties.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Paul Beiss, Properties of Powder Metallurgy Tool Steels, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 491–514, https://doi.org/10.31399/asm.hb.v07.a0006127
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Effects of Alloying on Powder Metallurgy Tool Steels
Powder Metallurgy
Chemical Composition of Powder Metallurgy High-Alloy Tool Steels
Powder Metallurgy
Microstructure of Powder Metallurgy Tool Steels
Powder Metallurgy
Workpiece Materials Database
Metalworking: Bulk Forming
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Introduction to Metals Process Simulation
Metals Process Simulation
2065 Aerospace Extrusion Alloy
Properties and Selection of Aluminum Alloys
Wear of Cast Irons
Friction, Lubrication, and Wear Technology
Nanofluids as Quenchants in Industrial Heat Treatment
Steel Heat Treating Technologies
Design for Powder Metallurgy
Materials Selection and Design