Joining Powder Metallurgy Steel Components[1]
Revising author
-
Published:2015
Abstract
This article characterizes the physical differences between powder metallurgy (PM) and wrought or cast materials, as they apply to joining. It discusses acceptable joining procedures and techniques, including welding and brazing and solid-state methods. Information on the weldability of various PM materials is presented. The article also describes the effects of porosity on several important properties that affect the welding characteristics.