Powder Metallurgy
Milling of Brittle and Ductile Materials[1]
Revising author
-
Published:2015
Abstract
Milling of materials, whether hard and brittle or soft and ductile, is of prime interest and of economic importance to the powder metallurgy (PM) industry. This article discusses the principles of milling, milling parameters, and the powder characteristics required for the process. It discusses the changes in powder particle morphology that occur during milling of metal powders produced by various processes such as microforging, fracturing, agglomeration, and deagglomeration. The article also provides useful information on milling equipment such as tumbler ball mills, vibratory ball mills, attrition mills, and hammer and rod mills.
Chris Schade, Milling of Brittle and Ductile Materials, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 77–87, https://doi.org/10.31399/asm.hb.v07.a0006089
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.