Infiltration of Carbide Structures
-
Published:2015
Abstract
This article provides information on the infiltration mechanism of carbide structures. It reviews the basic techniques used for metal infiltration, including dip infiltration, contact filtration, gravity feed infiltration, and external-pressure infiltration. The article highlights various applications of contact infiltration in oil, gas, and blast-hole drilling such as fixed-cutter drill bits and diamond-impregnated coring bits. It also discusses the applications of infiltrated carbide material in erosion-resistant cladding.
Anthony Griffo, Andrew Bell, Infiltration of Carbide Structures, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 726–728, https://doi.org/10.31399/asm.hb.v07.a0006099