The organizations that are most active in the development of standards for powder metallurgy (PM) are the American Society for Testing and Materials (ASTM), Metal Powder Industries Federation (MPIF), and International Standards Organization (ISO). This article presents the test method standards, materials standards, and material designation codes for PM materials. It provides information on the codes for structural parts, PM soft magnetic materials, PM self-lubricating bearings, metal injection molded materials, and powder forged materials.