Refractory metals are typically processed from powders into ingots that are subsequently swaged into round bars or rolled into plates. Secondary operations are required to fabricate more complex refractory metal components. This article discusses two such secondary operations, namely, machining and joining processes for tungsten, tungsten heavy alloys, molybdenum, tantalum, niobium, and rhenium components. It describes the various types of metal joining processes, including mechanical fastening, brazing, and welding.
Steven G. Caldwell, H. Kestler, N. Reheis, Secondary Operations and Quality Control for Refractory Metal Powders, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 620–624, https://doi.org/10.31399/asm.hb.v07.a0006133
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.