Powder Metallurgy
Pressing and Sintering of Refractory Metal Powders
-
Published:2015
Abstract
This article discusses the pressing and sintering of various refractory metal powders for the production of intermediate products as well as special cases of finished products. The metal powders considered include tungsten, molybdenum, tantalum, niobium and their alloys, as well as rhenium.
Sign in
ASM members
Member Sign InGerhard Leichtfried, John A. Shields, Jr., John L. Johnson, Pressing and Sintering of Refractory Metal Powders, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 605–610, https://doi.org/10.31399/asm.hb.v07.a0006124