This article discusses the production of aluminum and aluminum alloy powders with emphasis on the gas atomization method and the atomizing nozzle. It illustrates the particle formation mechanism and details the requisites for particle size distribution, control, and morphology. The article presents information on the mean oxide thickness formed on atomized powders. It also describes the mechanical and physical properties of aluminum and aluminum alloy powders, as well as their applications.

The powder metallurgy (PM) process is a relatively efficient and economic process that can be used to produce high quantities of aluminum components with a reasonable degree...