This article presents fractographs that show evidence of overload and fatigue in gray cast irons. The overload failure section illustrates a fractured motor housing, valve body, and bracket with microvoid coalescence (dimpled rupture) in the metal matrix between graphite flakes. The fractographs of fatigue failures illustrate a gearbox housing with fatigue striations and pearlitic microstructure.